Ангобована цегла — тип клінкера, на поверхню якого наноситься один шар шлікерної суспензії на першому етапі. Товщина цього шару становить не більше 0,5 мм. Далі така цегла відправляється в пічку. Далі повторюється перший етап знову і в результаті отримують цеглу з глянцевим блиском по боках. rdf:langString
Engineering bricks are a type of brick used where strength, low water porosity or acid (flue gas) resistance are needed. Engineering bricks can be used for damp-proof courses. Clay engineering bricks are defined in § 6.4.51 of British Standard BS ISO 6707-1;2014 (buildings & civil engineering works - vocabulary - general terms) as "fire-clay brick that has a dense and strong semi-vitreous body and which conforms to defined limits for water absorption and compressive strength" rdf:langString
rdf:langString Engineering brick
rdf:langString Ангобована цегла
xsd:integer 32971559
xsd:integer 1107473086
rdf:langString Engineering bricks are a type of brick used where strength, low water porosity or acid (flue gas) resistance are needed. Engineering bricks can be used for damp-proof courses. Clay engineering bricks are defined in § 6.4.51 of British Standard BS ISO 6707-1;2014 (buildings & civil engineering works - vocabulary - general terms) as "fire-clay brick that has a dense and strong semi-vitreous body and which conforms to defined limits for water absorption and compressive strength" Stronger and less porous engineering bricks (UK Class A) are usually blue due to the higher firing temperature whilst class B bricks are usually red. Class A bricks have a strength of 125 N/mm2 (18,100 lbf/sq in) and water absorption of less than 4.5%; Class B bricks have a strength greater than 75 N/mm2 (10,900 lbf/sq in) and water absorption of less than 7%. Accrington brick is a type of engineering brick that was used in the construction of the foundations in the Empire State Building.
rdf:langString Ангобована цегла — тип клінкера, на поверхню якого наноситься один шар шлікерної суспензії на першому етапі. Товщина цього шару становить не більше 0,5 мм. Далі така цегла відправляється в пічку. Далі повторюється перший етап знову і в результаті отримують цеглу з глянцевим блиском по боках.
xsd:nonNegativeInteger 2052

data from the linked data cloud